Add to Cart
Description | Closet Sliding Door Aluminum Profile T5 T6 6063 Aluminum Door Window Profile,Wood Color |
Material Thickness(t) | 1.0/1.1/1.2/1.4 mm |
Materiral | aluminum alloy 6063,6063A,6060,6061 |
Annealing Treatment | T3-T8 |
Color | Silver White ,Bronze , Champagne, Black, (RAL series)etc. |
Surface Treatment | anodized, powder coated, electrophoresis, wood grain, polished and etc |
Shape | Square, Round, Flat, Oval, and according to customer's drawing. |
Length | Normal length=6m or in customer's order |
Usage | Building, Production Line, Decoration, Industrial, Transportation, Door and window, etc. |
Package | 1. Pearl cotton foam for each profile; 2. Wrap with shrink film exterior; 3. Packed according to customer request. |
Advantages/Features | Providing colorful products with various mechanical performances to adapt all kinds of architectural styles |
Sliding aluminum doors, also called aluminum sliding door, are widely used as sliding closet doors, sliding cabinet doors, sliding bathroom doors, exterior sliding doors and sliding aluminum folding doors, and so on. They have beautiful appearance and smooth surface, and are wind proofing, water proofing, and anti-erosion.
1.20 years' experience and advanced equipment
2.Customize: We can manufacture according to your size and shape of such aluminum profile;
3.Strong production capacity - 28 extrusion lines, 50,000TONS/Year
4.One Stop Service Specialized in mould, extrusion, anodizing, powder coating, wood grain and Processing;
5.Shortest Delivery , competitive prices and excellent service
Aluminum Extrusion Advantages:
The extrusion process provides virtually unlimited opportunities for aluminium product shapes. Costs are cut by designing fewer components, which reduce fabrication and simplify assembly.
These features and benefits are unmatched by other materials and processes:
(1) Complex integral shapes
(2) Cost effective
(3) Low tooling costs
(4) Design flexibility
(5) V ersatility in joining
(6) Machinable
(7) Rapid prototyping
(8) Short lead times
(9)Wide range of finishes
Guangdong Yong long Aluminum Co., Ltd. is located in the No. 10 (Sanjiang market) of Leping Town, Sanshui District, Foshan. The company was founded in 1997. It is a comprehensive and large-scale aluminum profile enterprise integrating the research and development, production and sales of aluminum alloy profiles. The company is leading the "Hong Ying" brand. Strong comprehensive strength and excellent service make Yong long "Hong Ying" sell well all over the country and exported to Southeast Asia, Europe, South America ,South Africa and many other countries.
The company has 900 employees, including 120 high and intermediate engineering technology and management personnel, with advanced and perfect design, production, testing and testing methods as well as perfect sales network and after-sales service system. The products sell well in more than 10 national and foreign ports, Australia and Taiwan areas.
(1) select the substrate that has been sprayed or electrophoretic.
(2) use wood grain heat transfer paper to wrap the transferred substrate, and use the heat resistant adhesive tape to fix the interface of the paper, so as to prevent grained heat transfer paper from loosening. (Note: the front side of wood pattern heat transfer paper should be pasted with the transferred substrate.
(3)then set up the high temperature resistant and well sealed plastic plastic bag on the base material which has been wrapped by the wood grain heat transfer paper, and then vacuum from the two ends of the plastic bag until the plastic bag is fully and effectively cling to the base material. The negative pressure of vacuum should be adjusted according to the characteristics of the transferred substrate and the negative pressure that the plastic bag can bear, usually between 0.3 and 0.8Mpa. (Note: the purpose of using plastic bags is to force the wood grain hot transfer
paper to be fully and effectively pressed on the base material by the negative pressure.)
(4) the base material that has been wrapped is sent to the oven to bake. The height of the baking temperature and the length of the time should be adjusted according to the characteristics of the substrate, the depth of the transfer texture and the specific performance of the oven. The temperature of the transfer is usually 160~180 centigrade and the time is 5~8 minutes.
(5) remove the transferred substrate from the oven and pull out the plastic bag from one end of the transferred substrate (Note: this plastic bag can be reused), tearing down the hot transfer paper, and cleaning the surface.